Lithium Tantalate (LiTaO3)
Lithium tantalate (LiTaO3) is a high-performance electro-optic crystal widely used in electro-optic equipment, with good optical, nonlinear-optical and E-O properties and a high threshold described as a loss threshold. The supplier offers high-quality LiTaO3 crystals/wafers; the referenced table gives standard-use properties, with other specifications customizable. The description also states that LiNbO3 crystals, because of high electro-optic and acousto-optic coefficients, are widely used in Pockels cells, Q-switches, phase modulators, waveguide substrates and surface acoustic wave (SAW) applications. Other wafer sizes/specifications are available on request.
Overview
Specifications
| Parameter | Value |
|---|---|
| LiTaO3 Basic Properties - Crystal Structure | Trigonal, space group R₃c,Point group 3m |
| LiTaO3 Basic Properties - Lattice Parameters | a=5.154A,c=13.781A |
| LiTaO3 Basic Properties - Melting Point | 1650℃ |
| LiTaO3 Basic Properties - Curie Temperature | 607℃ |
| LiTaO3 Basic Properties - Mohs Hardness | 5.5 |
| LiTaO3 Basic Properties - Density | 7.46 g/cm³ |
| LiTaO3 Basic Properties - Dielectric Constant | ξ₁₁/ξ₀ 51.7;ξ₃₃/ξ₀ ₄₄.₅ |
| LiTaO3 Basic Properties - Elastic Stiffness Coefficient | C^E₁₁ 2.33(X 10¹¹ N/m²); C^E₃₃ 2.77(X 10¹¹ N/m²) |
| LiTaO3 Basic Properties - Piezoelectric Strain Constant | d₂₂ 2.4(X 10⁻¹¹ C/N); d₃₃ 0.8(X 10⁻¹¹ C/N) |
| LiTaO3 Basic Properties - Emission Range | 400-4500nm |
| LiTaO3 Basic Properties - Electro-Optic Coefficient | r₃₃ 30.4pm/V |
| LiTaO3 Basic Properties - Refractive Index (632.8nm) | nₒ=2.176,nₑ=2.180 |
| LiTaO3 - Standard SAW Properties - νₛ [X-112ᵒY] | 3295 m/s |
| LiTaO3 - Standard SAW Properties - κ²ₛ [X-112ᵒY] | 0.75 % |
| LiTaO3-SAW Standard Characteristics - TCV [X-112ᵒY] | -16.50 10⁻⁶/ᵒC |
| LiTaO3 - Standard SAW Properties - TCD [X-112ᵒY] | 22.3 10⁻⁶/ᵒC |
| LiTaO3 - Standard SAW Properties - νₛ [Y-Z] | 3230 m/s |
| LiTaO3 - Standard SAW Properties - κ²ₛ [Y-Z] | 0.66 % |
| LiTaO3 - Standard SAW Properties - TCD [Y-Z] | 35 10⁻⁶/ᵒC |
| LiNbO3 Basic Properties - Crystal Structure | Trigonal Crystal System, Space Group R₃c, Point Group 3m |
| LiNbO3 Basic Properties - Lattice Parameters | a=5.148A,c=13.863A |
| LiNbO3 Basic Properties - Melting Point | 1253℃ |
| LiNbO3 Basic Properties - Curie Temperature | 1140℃ |
| LiNbO3 Basic Properties - Mohs Hardness | 5 |
| LiNbO3 Basic Properties - Density | 4.64 g/cm³ |
| LiNbO3 Basic Properties - Dielectric Constant | ξ₁₁/ξ₀ 85;ξ₃₃/ξ₀ ₂₉.₅ |
| LiNbO3 Basic Properties - Elastic Stiffness Coefficient | C^E₁₁ 2.04(X 10¹¹ N/m²); C^E₃₃ 2.46(X 10¹¹ N/m²) |
| LiNbO3 Basic Properties - Piezoelectric Strain Constant | d₂₂ 2.04(X 10⁻¹¹ C/N); d₃₃ 19.22(X 10⁻¹¹ C/N) |
| LiNbO3 - Standard SAW Properties - νₛ [127.86ᵒY] | 3970 m/s |
| LiNbO3 - Standard SAW Properties - κ²ₛ [127.86ᵒY] | 5.5 % |
| LiNbO3 - Standard SAW Properties - TCV [127.86ᵒY] | -60 10⁻⁶/ᵒC |
| LiNbO3 - Standard SAW Properties - TCD [127.86ᵒY] | 78 10⁻⁶/ᵒC |
| LiNbO3 - Standard SAW Properties - νₛ [Y-X] | 3485 m/s |
| LiNbO3 - Standard SAW Properties - κ²ₛ [Y-X] | 4.3 % |
| LiNbO3 - Standard SAW Properties - TCV [Y-X] | -85 10⁻⁶/ᵒC |
| LiNbO3 - Standard SAW Properties - TCD [Y-X] | 95 10⁻⁶/ᵒC |
| Standard Diameter [LiTaO3; blank; diameter φ3”±2mm] | φ3"±2mm |
| Standard Diameter [LiTaO3; blank; diameter φ4”±2mm] | φ4"±2mm |
| Standard Length [LiTaO3; blank; diameter φ3”±2mm] | ≤120mm |
| Standard Length [LiTaO3; blank; diameter φ4”±2mm] | ≤100mm |
| Standard Orientation [LiTaO3; Blank] | 36°Y,42°Y |
| Diameter [LiTaO3; Wafer] | φ3"±2mm,φ4"±2mm |
| Thickness [LiTaO3; Wafer] | 0.3~1mm |
| Direction [LiTaO3; Wafer] | 36°Y,42°Y |
| Reference-Flat Orientation [LiTaO3; Wafer] | X |
| Reference-Flat Width [LiTaO3; Wafer] | 22±2 |
| Front-Surface Polish [LiTaO3; Wafer] | 0.25~0.016μm |
| Back-Surface Polish [LiTaO3; Wafer] | 10~15μm |
| Flatness [LiTaO3; Wafer] | ≤20 μm |
| Bow [LiTaO3; Wafer] | ≤30 μm |
| Standard Diameter [LiNbO3; blank; diameter φ3”±2mm] | φ3"±2mm |
| Standard Diameter [LiNbO3; blank; diameter φ4”±2mm] | φ4"±2mm |
| Standard Length [LiNbO3; blank; diameter φ3”±2mm] | ≤150mm |
| Standard Length [LiNbO3; blank; diameter φ4”±2mm] | ≤100mm |
| Standard Orientation [LiNbO3; Blank] | 127.86°Y,64°Y |
| Diameter [LiNbO3; Wafer; Diameter φ3 Inches ±2mm] | φ3"±2mm |
| Diameter [LiNbO3; Wafer; Diameter φ4 Inches ±2mm] | φ4"±2mm |
| Thickness [LiNbO3; Wafer; Diameter φ3 Inches ±2mm] | 0.5mm |
| Thickness [LiNbO3; Wafer; Diameter φ4 Inches ±2mm] | 1mm |
| Direction [LiNbO3; Wafer] | 127.86°Y,64°Y,47.5°Y,X,Y,Z |
| Reference-Flat Orientation [LiNbO3; Wafer] | X |
| Reference-Flat Width [LiNbO3; Wafer] | 22±2mm |
| Front-Surface Polish [LiNbO3; Wafer] | 0.25~0.016μm |
| Back-Surface Polish [LiNbO3; Wafer] | 10~15μm |
| Flatness [LiNbO3; Wafer; Diameter φ3 Inches ±2mm] | ≤30 μm |
| Flatness [LiNbO3; Wafer; Diameter φ4 Inches ±2mm] | ≤40 μm |
| Bow [LiNbO3; Wafer; Diameter φ3 Inches ±2mm] | ≤30 μm |
| Bow [LiNbO3; Wafer; Diameter φ4 Inches ±2mm] | ≤40 μm |
Datasheet
Please provide your email to download the datasheet.
Invalid email format. Please try again.
Supplier Information
Loading...
Name
Phone
Organization
Use Case

Database Platform