Ball-Tip Quartz Fiber QT-04
Ball-tip silica fiber is a special optical fiber with a spherical tip at one end. This design concentrates light emitted from, or collected into, the fiber end face. Ball-tip silica fibers are generally used for precise optical measurements and efficient optical-signal coupling. Silica offers excellent optical transparency and low optical loss, so these fibers are widely used in communications, medicine, and scientific research. Their manufacture involves precision processing. High-purity silica glass is first prepared and drawn into fiber. Specific heating and shaping methods, such as CO2 laser heating, then melt one end face into a spherical structure. Heating temperature and duration must be precisely controlled to meet the required tip shape and size. Main characteristics include low loss, high transmission efficiency, and good optical performance. Silica itself has a relatively low refractive index and damage threshold, allowing low-loss signal transmission over a broad wavelength range. The spherical tip further optimizes coupling efficiency and concentrates transmitted light, which is critical to overall fiber-system performance. Because of their distinctive structure and excellent optical performance, ball-tip silica fibers are widely used in multiple fields. In communication systems they can improve signal transmission efficiency and quality. In medicine they support precise optical imaging and laser surgery. They are also commonly used for optical measurement and precise signal control in research experiments.
Overview
Specifications
| Parameter | Value |
|---|---|
| Fiber End Face | Spherical |
| Fiber core diameter | 272 μm |
| Cladding Diameter | 299 μm |
| Coating Diameter | 330 μm |
| Buffer diameter | 420 μm |
| Length | 3M |
| Termination type | SMA905 |
| Numerical Aperture (NA) | 0.22 |
| Core Material | Low-OH Silica Material |
| Fiber cladding material | Fluorine-doped silica material |
| Coating Material | Acrylic resin |
| Buffer material | Teflon |
| Buffer color | Blue/green/black/white |
| Operating Temperature | -40℃~150ºC |
| Transmission wavelength | 400-2500nm/190-1100nm |
| Characteristics | Compliant with biocompatibility requirements |
| Proof-test strength | 100kpsi |
| Fiber Type | Step-index type |
Datasheet
Please provide your email to download the datasheet.
Invalid email format. Please try again.
Supplier Information
Loading...
Name
Phone
Organization
Use Case

Database Platform